UNS S31600 / S31603 · Austenitic stainless steel, molybdenum-bearing

SS 316 Fittings

Stainless Steel 316 / 316L fittings supplied to ASTM A403 WP316/316L and ASTM A182 F316/F316L from our Mumbai stockyard. SS 316 adds 2–3% molybdenum to the 18/8 base, which markedly improves resistance to pitting and crevice corrosion in chloride environments. It is the default grade for marine, coastal and chemical process service. 316L, the low-carbon variant, is specified for welded construction.

Ask on WhatsApp

Governing Standards for SS 316 Fittings

State the standard on your enquiry and we will confirm stock against it.

StandardCovers
ASTM A403 WP316/316LButtweld fittings
ASTM A182 F316/F316LForged fittings and flanges

SS 316 Chemical Composition (%)

Composition and mechanical values are the limits set by the governing ASTM specification and are given for reference. The mill test certificate supplied with your consignment carries the actual heat analysis.

Element316 (S31600)316L (S31603)
Carbon0.08 max0.030 max
Chromium16.0 – 18.016.0 – 18.0
Nickel10.0 – 14.010.0 – 14.0
Molybdenum2.00 – 3.002.00 – 3.00
Manganese2.00 max2.00 max
Silicon0.75 max0.75 max
Phosphorus0.045 max0.045 max
Sulphur0.030 max0.030 max
Technical Data

SS 316 Fittings Specifications

SS 316 Fittings — Chemical Composition

Chemical Composition for SS 316 Fittings supplied by Ritvik Metal Impex
GradeCMnPSSiCrNiMoOther
TP 3040.082.000.0450.0301.0018.0–20.08.0–11.0—N 0.10
TP 304L0.0352.000.0450.0301.0018.0–20.08.0–13.0—N 0.10
TP 3160.082.000.0450.0301.0016.0–18.011.0–14.02.00–3.00N 0.10
TP 316L0.0352.000.0450.0301.0016.0–18.010.0–15.02.00–3.00N 0.10
TP 3210.082.000.0450.0301.0017.0–19.09.0–12.0—Ti ≥ 5 × C
TP 3470.082.000.0450.0301.0017.0–19.09.0–13.0—Nb ≥ 10 × C
TP 310S0.082.000.0450.0301.0024.0–26.019.0–22.0——
TP 317L0.0352.000.0450.0301.0018.0–20.011.0–15.03.00–4.00N 0.10

Note: Per ASTM A312 / A240. Values are maximum % by weight unless a range is shown. ASTM A312 permits 0.035% max carbon on L grades, where ASTM A240 plate specifies 0.030% max.

Values shown are the specified minima and maxima published in the governing standards and are given for guidance. The mill test certificate supplied with your consignment reports the actual results for that heat.

When to specify SS 316 for fitting work

Choose 316 or 316L wherever chlorides are present — coastal installations, seawater cooling, brines, bleaches and many process chemicals — and in pharmaceutical and food plant where aggressive cleaning chemicals are used. If chloride levels or temperatures are higher still, or if higher strength would allow a lighter section, consider Duplex 2205.

Products in this range

SS 316 in other forms

Full composition, properties and equivalents on the Stainless Steel 316 / 316L grade page.

Frequently Asked Questions

Is 316 always better than 304?
Better in chlorides, not universally. The molybdenum in 316 buys pitting resistance and costs roughly 25–40% more. In dry indoor service, freshwater or architectural work away from the coast, 304 performs identically and specifying 316 simply raises the bill. Choose on the environment, not on the grade number.
What does the "L" mean and when do I need it?
L denotes low carbon — 0.030% maximum instead of 0.08%. It matters when the component is welded: lower carbon suppresses chromium carbide precipitation in the heat-affected zone and protects against intergranular attack. For welded pipe, fittings and fabricated assemblies specify 316L. Dual-certified 316/316L material, which meets both, is common and usually the practical choice.