UNS S30400 / S30403 · Austenitic stainless steel

SS 304 Sheets, Plates & Coils

Stainless Steel 304 / 304L sheets, plates & coils supplied to ASTM A240 from our Mumbai stockyard. SS 304 is the most widely used stainless steel: an 18/8 austenitic grade with good corrosion resistance in atmospheric, freshwater and mild chemical service, excellent formability and straightforward welding. 304L, the low-carbon variant, is specified where the part is welded and heavy sections risk sensitisation.

Ask on WhatsApp

Governing Standards for SS 304 Sheets, Plates & Coils

State the standard on your enquiry and we will confirm stock against it.

StandardCovers
ASTM A240Plate, sheet and coil

SS 304 Chemical Composition (%)

Composition and mechanical values are the limits set by the governing ASTM specification and are given for reference. The mill test certificate supplied with your consignment carries the actual heat analysis.

Element304 (S30400)304L (S30403)
Carbon0.08 max0.030 max
Chromium18.0 – 20.018.0 – 20.0
Nickel8.0 – 10.58.0 – 12.0
Manganese2.00 max2.00 max
Silicon0.75 max0.75 max
Phosphorus0.045 max0.045 max
Sulphur0.030 max0.030 max
Nitrogen0.10 max0.10 max
Technical Data

SS 304 Sheets, Plates & Coils Specifications

SS 304 Sheets, Plates & Coils — Chemical Composition

Chemical Composition for SS 304 Sheets, Plates & Coils supplied by Ritvik Metal Impex
GradeCMnPSSiCrNiMoOther
TP 3040.082.000.0450.0301.0018.0–20.08.0–11.0—N 0.10
TP 304L0.0352.000.0450.0301.0018.0–20.08.0–13.0—N 0.10
TP 3160.082.000.0450.0301.0016.0–18.011.0–14.02.00–3.00N 0.10
TP 316L0.0352.000.0450.0301.0016.0–18.010.0–15.02.00–3.00N 0.10
TP 3210.082.000.0450.0301.0017.0–19.09.0–12.0—Ti ≥ 5 × C
TP 3470.082.000.0450.0301.0017.0–19.09.0–13.0—Nb ≥ 10 × C
TP 310S0.082.000.0450.0301.0024.0–26.019.0–22.0——
TP 317L0.0352.000.0450.0301.0018.0–20.011.0–15.03.00–4.00N 0.10

Note: Per ASTM A312 / A240. Values are maximum % by weight unless a range is shown. ASTM A312 permits 0.035% max carbon on L grades, where ASTM A240 plate specifies 0.030% max.

Values shown are the specified minima and maxima published in the governing standards and are given for guidance. The mill test certificate supplied with your consignment reports the actual results for that heat.

When to specify SS 304 for plate work

Choose 304 for general corrosion resistance, food and dairy contact, architectural work and indoor process piping. Move up to 316 when chlorides are present — seawater, coastal air, brines or chlorinated cleaning chemicals — because 304 is vulnerable to pitting in those conditions.

Products in this range

SS 304 in other forms

Full composition, properties and equivalents on the Stainless Steel 304 / 304L grade page.

Frequently Asked Questions

What is the difference between 304 and 304L?
304L limits carbon to 0.030% against 0.08% for 304. The lower carbon reduces the risk of chromium carbide precipitation at grain boundaries during welding — sensitisation — which would otherwise leave the heat-affected zone vulnerable to intergranular corrosion. Specify 304L for welded heavy sections; 304 is adequate for thin sections and non-welded parts. 304L has slightly lower strength as a result.
Is SS 304 suitable for seawater?
No. Chlorides attack the passive layer on 304 and cause pitting and crevice corrosion. For seawater and chloride-bearing service use 316/316L, and for higher chloride levels or higher temperatures use Duplex 2205 or a super duplex grade.
SS 304 Sheets, Plates & Coils Enquiry

Send your SS 304 Sheets, Plates & Coils requirement

Give us the size, schedule or thickness, quantity and standard and we will confirm stock and send a firm price. Minimum order quantity 5 kg, mill test certificate to EN 10204 3.1 with every consignment.